ADVANCED MATERIALS & PROCESSES •
SEPTEMBER 2014
26
hensive Treatment
, Vol 19B, Corrosion and Environmental
Degradation of Materials, Wiley-VCH, Weinheim, Ger-
many, p 229-325, 1999.
5. R. Darolia and W.S. Walston, Development and Charac-
terization of High Strength NiAl Single Crystal Alloys,
Structural Intermetallics,
1997, M.V. Nathal, et al., eds.,
TMS, Warrendale, PA, p 585-94, 1997.
6. R.R. Judkins and U.S. Rao, Fossil Energy Applications of
Intermetallic Alloys,
Intermetallics,
Vol 8, p 1347-1354,
2000.
7. B.A. Pint, et al., Mechanistic-Based Lifetime Predictions
for High Temperature Alloys and Coatings,
JOM,
Vol 64,
p 1454-1460, 2012.
8. Y. Yamamoto, et al., Alumina-Forming Austenitic Stain-
less Steels Strengthened by Laves Phase and MC Carbide
Precipitates,
Metall. Mater. Trans. A,
Vol 38, p 2737-2746,
2007.
9. D.M. Dimiduk and J.H.Perepezko, Mo-Si-B Alloys: De-
veloping a Revolutionary Turbine-Engine Material,
MRS
Bulletin,
Vol 28, p 639-645, 2003.
10. B.P. Bewlay, et al., A Review of Very-High-Temperature
Nb-Silicide-Based Composites,
Metall. Mater. Trans. A,
Vol 34, p 2043-2052, 2003.
11. R. Sakidja, et al., Phase Stability and Structural Defects
in High-Temperature Mo-Si-B Alloys,
Acta Mater.,
Vol 56,
p 5223–5244, 2008.
12. J.H. Perepezko, The Hotter the Engine, the Better,
Sci-
ence,
Vol 326, p 1068-1069, 2009.
13. J.A. Lemberg and R.O. Ritchie, Mo-Si-B Alloys for Ul-
trahigh-Temperature Structural Applications,
Advanced
Materials,
Vol 24, p 3445-3480, 2012.
14. M. Middlemas and J.K. Cochran, Dense Fine-Grain
Mo-Si-B Alloys from Nitride-Based Reactions,
JOM,
Vol
60, p 19-24, 2008.
15. M. Krüger, et al., Mechanically Alloyed Mo-Si-B Alloys
with a Continuous α-Mo Matrix and Improved Mechani-
cal Properties,
Intermetallics,
Vol 16, p 933-941, 2008.
16. G. Hasemann, et al., Microstructure and Creep Proper-
ties of a Near-Eutectic Directionally Solidified Multiphase
Mo-Si-B Alloy,
Intermetallics,
Vol 48, p 28-33, 2014.
17. S. Miyamoto, et al., Phase Equilibria, Microstructure
and High-Temperature Strength of TiC-Added Mo-Si-B
Alloys,
Metall. Mater. Trans. A,
Vol 45, p 1112-1123, 2014.
18. F.A. Rioult, et al., Transient Oxidation of Mo-Si-B Al-
loys: Effect of the Microstructure Size Scale,
Acta Mater.,
Vol 57, p 4600-4613, 2009.
19. J.H. Perepezko and R. Sakidja, Oxidation Resistant
Coatings for Ultrahigh Temperature Refractory Mo-Base
Alloys,
Adv. Eng. Mater.,
Vol 11, p 892-897, 2009.
20. J.H. Perepezko and R. Sakidja, Extended Functionality
of Environmentally-Resistant Mo-Si-B-Based Coatings,
JOM,
Vol 65, p 307-317, 2013.
21. S. Knittel, et al., Development of Silicide Coatings to
Ensure the Protection of Nb and Silicide Composites
Against High Temperature Oxidation,
Surf. Coat. Tech.,
Vol
235, p 401-406, 2013.




