Fig. 5
Same recipe 72 h after Fig. 4
Fig. 6
20:1 iodic acid
Fig. 7
30:1 iodic acid
Fig. 8
40:1 iodic acid
Fig. 9
20:1 iodic acid in dilute nitric acid
Fig. 10
30:1 iodic acid in dilute nitric acid