A D V A N C E D M A T E R I A L S & P R O C E S S E S | F E B R U A R Y 2 0 1 6
8
The researchers’ aluminum oxide plates
are 1000× thinner than a sheet of paper,
but can be squeezed and bent without
breaking. Courtesy of Bargatin Group.
to preventing curling, the corrugation
resists tearing by stopping cracks at an
internal wall.
upenn.edu.
www.masterbond.com Hackensack, NJ 07601 USA +1.201.343.8983 • main masterbond.com • High temperature resistance • Resists a wide variety of chemicals • Outstanding thermal cycling capabilities Toughened Epoxy Supreme 42HT-2with The Boeing Co., Chicago, valued
at over $2.5 billion. Under the agree-
ments, Alcoa Fastening Systems & Rings
will supply advanced titanium, stainless
steel, alloy steel, aluminum, and nick-
el-base superalloy fastening systems for
every Boeing platform, and Alcoa will
serve as the sole supplier of ready-to-in-
stall titanium seat track assemblies for
Alcoa will supply titanium seat track assemblies for the entire 787 Dreamliner family, includ-
ing the 787-9 shown here. Courtesy of Boeing.
all three 787 Dreamliner variants. Titani-
um seat tracks are stronger, weigh less,
and offer superior corrosion resistance
compared with traditional materials. Al-
coa will supply tracks using production
capabilities gained through the acqui-
sition of RTI International Metals. RTI is
now known as Alcoa Titanium & Engi-
neered Products.
alcoa.com.
AEROSPACE COMPOSITE
EARNS SAE-AMS
SPECIFICATION
The Society of Automotive En-
gineers—Aerospace Material Specifi-
cation Nonferrous Alloys Committee
(SAE-AMS) published aerospace speci-
fication AMS4355 for SupremEX 225XE,
a particle-reinforced, aerospace-grade
aluminum metal matrix composite
produced by Materion Corp., Mayfield
Heights, Ohio. SupremEX 225XE is made
by reinforcing a high-quality aerospace
aluminum alloy with 25 vol% ultrafine
silicon carbide particles, resulting in a
lightweight, strong, and stiff composite
that can replace aluminum, titanium,
steel, and other structural alloys and
composites. The AMS4355 specifica-
tion covers the material in reinforced,
hot isostatically pressed shaped billets.
Materion is working to obtain specifi-
cations for forged and extruded forms,
and other grades of the SupremEX
product line.
materion.com.
ALCOA AND BOEING
FORGE SUPPLY DEALS
Alcoa Inc., Pittsburgh, recently
signed two long-term supply contracts