April_AMP_Digital

A D V A N C E D M A T E R I A L S & P R O C E S S E S | A P R I L 2 0 1 8 3 0 TECHNICAL SPOTLIGHT ION MILLING MAXIMIZES EBSD SENSITIVITY FOR STUDYING METALLOGRAPHIC SAMPLES Because electron backscatter diffraction is a surface-sensitive technique, preparing the sample surface so that it is smooth and free of defects is crucial to successful analysis. E lectron backscatter diffraction (EBSD) is a scanning electron mi- croscope (SEM)-based analytical technique that provides a wealth of in- formation regarding the microstructure of thematerial under study [1] . Newmicro- analysis instrumentation and software now enables scientists and researchers to conduct experiments using this tech- nique and generate valuable information, quickly and clearly. EBSD involves direct- ing a focused beamof electrons at a sam- pleof interest,which is tiltedat a70° angle in order to maximize backscattered elec- trons. The atomic planes in the material inelastically scatter these electrons when they satisfy the Bragg equation, diffract- ing them in such a way as to form a set of paired large angle cones corresponding to the diffracting plane. When projected onto a 2D phosphor screen, pairs of lines of distinct intensity are formed, giving rise to the characteristic Kikuchi bands for the EBSDpattern. An example of the resulting diffraction pattern is shown in Fig. 1. The Kikuchi bands in the diffrac- tion pattern are characteristic of the crystal structure under study. First, the distance between the bright lines forming each Kikuchi band is inverse- ly proportional to the spacing of the atomic plane from which the electron was diffracted. Next, the intersections of the bands correspond to the zone axes in the crystal. The angle between these intersecting lines provides the in- formation needed to determine crys- tal orientation. Finally, the intensity of the Kikuchi bands is a function of the fractional representation of the atom- ic planes contributing to the back- scattered diffraction pattern and the relative mass of the atom, which is im- portant when indexing materials com- posed of different elements. An accurate analysis of the materi- al microstructure requires a high degree of confidence in Kikuchi band detection, which in turn requires a high-quality dif- fraction pattern. Because the technique depends entirely on the top 10–15 nm of the material, optimizing the surface preparation is essential to achieving a high-quality diffraction pattern. SAMPLE POLISHING METHODS Polishing samples by hand on a rotating polishing wheel is a low cost, straightforward method to prepare the sample surface for EBSD analysis. De- tails regarding polishing best practices are thoroughly explained by metallur- gical engineer George Vander Voort and are available on his website [2] . In gen- eral, the sample is first rough-polished with sand paper at successively finer grits—200, 400, and 800—to achieve a generally flat and smooth surface. Next, the sample is fine polished with a se- ries of slurries of successively small- er grinding particulates—9, 3, 1, and 0.25 microns—to create a surface free of scratches and imperfections. The sam- ple can be finished with a gentle polish in a 0.020 micron slurry or vibrated in a colloidal solution to remove any sub- surface strain. Hand polishing is a highly effective technique for preparing most samples for EBSD analysis when the procedure is carefully followed. A Euler map is a common way to represent the distribu- tion and orientation of the grains with- in the region of the sample analyzed [3] . Figure 2 shows the resulting Euler map from a properly polished nickel sample. When proper technique is not ad- hered to—or equipment is poorly main- tained—results such as those in Fig. 3 can be expected. The electron image of the sample demonstrates that strong, Fig. 1 — Characteristic Kikuchi bands form the typical EBSD diffraction pattern. Fig. 2 — Euler map of a properly polished nickel sample.

RkJQdWJsaXNoZXIy MjA4MTAy