37
31
34
METALLURGY LANE
THE DECLINE OF THE
INTEGRATED STEEL
INDUSTRY—PART II
Charles R. Simcoe
The U.S. steel industry began its steady
decline in the late 1950s, a devastation
of epic proportions that continued
throughout the 1980s and beyond.
WILLIAMFRAZIER:
2016-2017 PRESIDENT OF
ASM INTERNATIONAL
Meet William E. Frazier, FASM, the new
president of ASM.
ASM NEWS
The monthly publication about ASM
members, chapters, events, awards,
affiliates, and other Society activities.
DEVELOPINGSTRONGCORE TECHNOLOGY
FORHIGHPRESSURE DIE CASTING
Frank Czerwinski, Gabriel Birsan, Frank Benkel, Wojciech Kasprzak, Mike
Walker, Jock Smith, Douglas Trinowski, and Ignacio Musalem
A new technology is needed in order to manufacture certain lightweight automotive com-
ponents, in particular those with hollow structures of complex geometry.
18
A D V A N C E D M A T E R I A L S & P R O C E S S E S | J A N U A R Y 2 0 1 7
2
Engine block produced using
precision sand and high
pressure die casting. Courtesy of
GM Research and Development
Center.
On The Cover: