August_EDFA_Digital

edfas.org ELECTRONIC DEVICE FAILURE ANALYSIS | VOLUME 20 NO. 3 26 TEM analysis revealed the root cause: The tungsten plug penetrates the nickel silicide layer due to a hole in this layer (Fig. 3). CASE #2: INCREASED SUBSTRATE LEAKAGE Corner experiments of the contact etch process showed that contacts had punched through the SiGe interlayer system (Fig. 3). Current imagingwas performed in order to characterize the electrical impact caused by this defect. Additional transistor probing experiments were performed to confirm the CI results. The test structure consists of a continuous contact chain between silicided P-active island with a SiGe inter- layer and metal 1. The vertical contacts are tungsten plugswith a TiNdiƒusion barrier layer. The SiGe interlayer systembelongs to the strain engineering features of PMOS transistors inmodern technologies. For the purpose of the experiment, the wafer was taken from production before metal 1 processing in order to have the contacts at the sample surface. The image generated when applying a bias of - 1.5 V to the sample while reading the current at the probe tip showed contacts of very similar brightness (Fig. 4). In contrast, applying a bias of + 1.5 V to the sample while scanning the same area reveals notable differ- ences in the brightness of various spots, i.e., their current response (Fig. 5). Using the detailed scan shown in Fig. 5 (bottom), the probe tip can be positioned on the various contacts without the need to un-blank the electron beam. This helps to reduce the sample’s exposure to the electron beam and thus minimize surface contamination. Using the needle already in contact with the sample, IV measurements were performed on two of the con- tacts—one showing a strong current response and one showing a weak response. The obtained IV curves show Fig. 4 Sample bias -1.5 V. Fig. 3 TEM analysis of fault in via chain showing a punch through the SiGe interlayer system. Fig. 5 Sample bias 1.5 V (top), zoomed area (bottom).

RkJQdWJsaXNoZXIy MjA4MTAy