April_AMP_Digital
A D V A N C E D M A T E R I A L S & P R O C E S S E S | A P R I L 2 0 1 8 7 ASM SUPERHERO VETS VIBRANIUM The latest Marvel Studios film “Black Panther” hit the big screen on February 16 and once again showcased the fictional supermaterial vibranium. Previously, in the 2016Marvel film“Cap- tain America: Civil War,” Black Panther demonstrated his powers by leaving scratches on Captain America’s nearly indestructible shield. This makes sense because Black Panther’s suit and weap- ons and Captain America’s shield are all made of vibranium, which is only available in Black Panther’s kingdom of Wakanda. Vibranium is a fictional me- tallic element that can store and release energy, making it a highly versatile ma- terial in Marvel’s cinematic universe. For more details on both real and imagined strategic materials, ASM su- perhero Suveen Mathaudhu, FASM, frequently speaks about the scientific phenomena underpinning various ele- ments such as vibranium. Mathaudhu, assistant professor of materials science and mechanical engineering at the University of California, Riverside, also addresses the complex global issues in strategic materials availability for ad- vanced technologies. As an avid comic book and superhero fan, Mathaudhu regularly provides scientific consult- ing to the entertainment industry. An OMG! OUTRAGEOUS MATERIALS GOODNESS many titanium alloys. “This new way to treat wood makes it 12 times stronger than natural wood and 10 times tough- er,” says research leader Liangbing Hu of UMD’s A. James Clark School of En- gineering. “This could be a competitor to steel or even titanium alloys. It’s also comparable to carbon fiber, but much less expensive. This kind of wood could be used in cars, airplanes, buildings— any application where steel is used.” The team also tested the new wood material and natural wood by shooting bulletlike projectiles at it. The projectile blew straight through the natural wood while the treated wood stopped the projectile partway through. “The most outstanding observa- tion, in my view, is the existence of a limiting concentration of lignin, the glue between wood cells, to maximize the mechanical performance of the densified wood. Too little or too much removal lowers the strength compared to a maximum value achieved at inter- mediate or partial lignin removal. This reveals the subtle balance between hydrogen bonding and the adhesion imparted by such a polyphenolic com- pound. Moreover is the fact that wood densification leads to both increased strength and toughness, two properties that usually offset each other,” explains Orlando Rojas, a professor at Aalto Uni- versity in Finland. umd.edu . active panelist at comic conventions, he recently appeared on a StarTalk Live! panel at AwesomeCon/Smithso- nian FutureCon with the late great Ste- phen Hawking to discuss advanced ma- terials capable of taking humanity to Mars and beyond. “Vibranium as a structural and functional material offers the epito- me of materials advancement. In the same way that Black Panther’s suit can both protect him and provide power for his feats, future vehicles could be made with structural frames that are also batteries, allowing them to col- lect from renewable energy sources,” says Mathaudhu. “As scientists and en- gineers, we are trying to develop real metallic materials that mimic these properties.” For more information: smathaudhu@engr.ucr.edu , www.ucr.edu . TIMBER AS STRONG AS TITANIUM Engineers at the Uni- versity of Maryland, Col- lege Park (UMD) recently discovered how to make wood more than 10 times stronger and tougher than ever before, creating a natural substance that is reportedly stronger than From left, Liangbing Hu and Teng Li discovered a way to make woodmore than 10 times stronger and tougher than ever before. Courtesy of UMD. From left, the Black Panther and ASM superhero Suveen Mathaudhu, FASM. Panther image courtesy of Walt Disney Studios Motion Pictures.
Made with FlippingBook
RkJQdWJsaXNoZXIy MjA4MTAy