1 8 S T R U C T U R A L M A T E R I A L S Among the structural materials developed in the 20th century, titanium and its alloys have played a leading role in improving component performance. *Member of ASM International Francis H. (Sam) Froes, FASM,* Consultant Ashraf Imam, George Washington University TITANIUM: A HISTORIC AND CURRENT PERSPECTIVE PART II