May_EDFA_Digital

edfas.org ELECTRONIC DEVICE FAILURE ANALYSIS | VOLUME 20 NO. 2 52 LITERATURE REVIEW T he current column covers peer-reviewed articles published since 2015 on reverse engineering, counterfeit electron- ics, case studies, system level, and packaging. All of these fields are dependent on failure analysis for their success. Note that inclusion in the list does not vouch for the article’s quality, and category sorting is by no means strict. If you wish to share an interesting recently published peer-reviewed article with the community, please forward the citation to the email address listed above and I will try to include it in future installments. Entries are listed in alphabetical order by first author, then title (in bold), journal, year, volume, and first page. Note that in some cases bracketed text is inserted into the title to provide clarity about the article subject. Peer-Reviewed Literature of Interest to Failure Analysis: Reverse Engineering, Counterfeit Electronics, Case Studies, System Level, and Packaging Michael R. Bruce, Consultant mike.bruce@earthlink.net • TM. Alam, H. Shen, N. Asadizanjani, et al.: “Impact of X-Ray Tomography on the Reliability and [Counterfeit Detection] of Integrated Circuits,” IEEE Trans. Dev. Mater. Reliab., 2017, 17, p 59. • A. Bazzazi, M.T.M. Shalmani, A.M.A. Hemmatyar: “Hardware Trojan Detection Based on Logical Testing,” J. Electron. Test., 2017, 33, p 381. • J. Breier, W. He, S. Bhasin, et al.: “Extensive Laser Fault Injection [Attack] Profiling of 65 nm FPGA,” . J Hardw. Syst. Secu., 2017, https://doi.org/10.1007/ s41635-017-0016-z. • C. Chen, S. Nagao, H. Zhang, et al.: “Mechanical Deformation of Sintered Porous Ag Die Attach at High Temperature and Its Size Effect for Wide- Bandgap Power Device Design,” J. Electron. Mater., 2017, 46, p 1576. • C.Q.Chen,G.B.Ang,J.Lam,etal.: “EmbedSRAMIDDOFF Fail Root Cause Identification by Combination of Device Analysis and Localized Circuit Analysis,” Microelectron. Reliab., 2017, 76-77, p 261. • W.J. Chen, Y.L. Lee, T.Y. Wu, et al.: “Effects of Electrical Current andExternal Stress on the Electromigration of Intermetallic Compounds between the Flip-Chip Solder and Copper Substrate,” J. Electron. Mater., 2018, 47, 35. • S. Cheng, C.-M. Huang, M. Pecht: “A Review of Lead-Free Solders for Electronics Applications,” Microelectron. Reliab., 2017, 75, 77. • H. Conseil-Gudla, M.S. Jellesen, R. Ambat: “Printed Circuit Board Surface Finish and Effects of Chloride Contamination, Electric Field, andHumidity on Cor- rosion Reliability,” J. Electron. Mater., 2017, 46, p 817. • M. Deluca, Hammer, J. Keckes, et al.: “Integrated Experimental and Computational Approach for Residual Stress Investigation near Through-Silicon Vias,” J. Appl. Phys., 2016, 120, p 195104. • F. Faggin: “Reverse Engineering: How We Made the [Intel] Microprocessor,” Nat. Electron., 2018, 1, p 88. • M. Fakharzadeh and M. Tazlauanu: “Methods for Failure Analysis and Diagnosis of Millimeter-Wave System-in-Packages,” IEEE Trans. Dev. Mater. Reliab., 2017, 17, p 371. • J.P. Gambino, S.A. Adderly, J.U. Knickerbocker: “An Overview of Through-Silicon via Technology and Manufacturing Challenges [Review],” Microelectron. Eng., 2015, 135, p 73. • E. George and M. Pecht: “RoHS Compliance in Safety and Reliability Critical Electronics,” Microelectron. Reliab., 2016, 65, p 1. • C.M. Huang, D. Nunez, M. Pecht, et al.: “Risk of Tin Whiskers in the Nuclear Industry,” Microelectron. Reliab., 2018, 81, p 22. • J.R. Kermode, A. Gleizer, G. Kovel, et al.: “Low Speed Crack Propagation via Kink Formation and Advance on the Silicon (110) Cleavage Plane,” Phys. Rev. Lett., 2015, 115, p 135501. • Y. Li, O. Hatch, P. Liu, et al.: “Root Cause Investigation of Lead-Free Solder Joint Interfacial Failures After Multiple Reflows,” J. Electron. Mater., 2017, 46, p 1674. • Y. Li, P.K.M. Srinath, D. Goyal: “A Review of Failure Analysis Methods for Advanced 3D Microelectronic Packages,” J. Electron. Mater., 2016, 45, p 116.

RkJQdWJsaXNoZXIy MjA4MTAy