May_EDFA_Digital
edfas.org ELECTRONIC DEVICE FAILURE ANALYSIS | VOLUME 20 NO. 2 46 BRUKER DEBUTS NANOMECHANICS LAB Bruker Corp., Billerica, Mass., announces the NanoMechanics Lab, a suite of force-mapping modes that enable Dimension FastScan and Icon AFM systems to performquantitative nanoscale characterization, extend- ing from soft hydrogels and polymers to stiff metals and ceramics. The NanoMechanics Lab encompasses a broad range of nanoscale AFMmeasurement techniques, includ- ing thewell-established force volumemode, aswell as the new high-accuracy PeakForce QNM, FASTForce volume, and FASTForce volume contact resonance modes. Using advanced algorithms and AFM probe manufacturing methods, these modes deliver repeatable and accurate high-volume quantitative measurements, with the addi- tion of data cubes for multidimensional nanoscale analy- sis of materials. For more information, visit bruker.com . HORIBA SCIENTIFIC INTRODUCES UVISEL PLUS Horiba Scientific, Japan, a global leader in spectro- scopic ellipsometry for over 25 years, announces the launchof Uvisel Plus, amodular ellipsometer that includes acquisition technology designed to measure thin-film samples faster and more accurately than ever. FastAcq, thecompany’snewest acquisition technology, is based on double modulation designed for real-world thin-film characterization. Based on a new electronic data-processing and high-speed monochromator, the FastAcq technology enables a samplemeasurement from 190 to 2100 nm to be completed within three minutes at high resolution. The ability to continuously adjust the spectral resolution along themeasurement range enables smarter and faster sample scanning. The Uvisel Plus also introduces a new calibration procedure, delivering faster performance and accuracy. Due to its design, which has no rotating elements and no additional components in the optical path, the Uvisel series phase-modulation technology delivers pure and efficient polarizationmodulation for accurate ellipsomet- ric parameter measurements. The superior polarization modulation capabilities of the photoelastic modulator deliver the highest sensitivity for measurement of critical thin, transparent layers deposited onto glass substrates. Designed for enhanced flexibility for thin-filmmeasure- ments, the Uvisel Plus offers microspots for patterned samples down to 50 µm, variable angles from 40° to 90°, an automatic horizontal mapping stage, and a variety of accessories, making it scalable to meet numerous appli- cation and budget needs. The spectral range from 190 to 2100 nm is covered by two Uvisel Plus configurations: 190 to 920 nm and a near-infrared extension to 2100 nm. The easy upgradability is a hallmark of the Uvisel Plus tomeet ongoing demanding applications. Driven by an advanced DeltaPsi2 software platform, as well as the Auto-Soft interface featuring an intuitiveworkflow to speed up data collection and analysis, the Uvisel Plus allows users from novice to expert to perform thin-filmmeasurements with extremely high accuracy and sensitivity. For more information, visit horiba.com/uviselplus. NEWMICROSCOPY TECHNIQUE REPORTED FOR NANOMECHANICAL SUBSURFACE IMAGING Northwestern University, Evanston, Ill., reports the development of scanning near-field thickness resonance acoustic microscopy (SNTRAM), an imaging technology with sharp phase contrast and mechanical sensitivity that suits awide range of applications in nanomechanical imaging of semiconductor structures and othermaterials. Acousticwaves canbe used tomeasure several proper- ties, such as thickness, sound speed, acoustic impedance, density, bulk modulus, and attenuation for numerous materials, both soft and hard. Because these are elastic strain waves that can travel through different materials without causing any damage, they canbeused for imaging subsurface structures noninvasively, a concept widely used in medical imaging. Nanoscale spatial resolution Horiba’s Uvisel Plus.
Made with FlippingBook
RkJQdWJsaXNoZXIy MjA4MTAy