May_EDFA_Digital
edfas.org ELECTRONIC DEVICE FAILURE ANALYSIS | VOLUME 20 NO. 2 18 DIAGNOSTIC TECHNIQUE SELECTION FOR SRAM LOGIC TYPE FAILURES Zhigang Song and Laura Safran GlobalFoundries, Hopewell Junction, N.Y. zhigang.song@globalfoundries.com EDFAAO (2018) 2:18-24 1537-0755/$19.00 ©ASM International ® INTRODUCTION Static random access memory (SRAM) is often chosen as the process qualification vehicle during technology development, and consequently, failure analysis of SRAM is the main feedback for process improvement and yield learning. [1,2] Because SRAM is very dense and has small features, its functionality is highly sensitive to process variation. Another advantage of using SRAM as a process qualification vehicle is that single-bit failure and many multi-bit failures can be precisely localized by a functional test and are easy for physical failure analysis. Generally, the defect causing a single-bit failure is precisely located at the failing bit site. In the case of paired-bit or quad-bit failures, the defect is often found at their shared stacked interconnects. For such failures, the passive voltage con- trast (PVC) technique, [3] scanning electron microscope (SEM) inspection, focused ion beam (FIB) cross-section, and electrical probing by atomic force probe [4] or SEM in- chamber probe [5] canbe employed to locate and image the defect. Since SRAM is organized as an array structure of single-bit storage cells, which are accessed and selected through the hierarchy bit-line (BL) and word-line (WL) decoder schemes, any defect in the address decoder circuitry will result in a uniquely failing spatial pattern. In general, these spatially patterned failures can be classi- fied into three categories, namely bit-line, word-line, and entire block failure. It is also worth noting that inmodern SRAM designs, the entire array becomes vulnerable to a defect within the control scan chain. A defect within such circuitrymay cause thewhole SRAMdevice tomalfunction or may prevent functional testing of the array. In this article, SRAM failures caused by defects in the address decoder or scan chain circuitry are categorized as SRAM logic type failures. Conventional failure analy- sis methods for single and multiple-bit failures are not effective for these types of failures. Consequently, more detailed fault isolation work is required prior to starting destructive physical failure analysis. Many diagnostic techniques such as photon emissionmicroscopy (PEM), [6,7] thermally induced voltage alteration (TIVA), [8,9,10] optical beam induced resistance change (OBIRCH), [8,11] critical parameter analysis (CPA) [12,13] and laser voltage imaging (LVI) [14,15] /laser voltage probing (LVP) [16,17] are available for the fault isolation work. These techniques offer alterna- tives for stimulating the SRAM device and detecting a response, and therefore provide a means for localizing a variety of faults for different failure types. Thus, select- ing the right diagnostic technique for a particular SRAM logic failure is important for an efficient and success- ful analysis. COMMON DIAGNOSTIC TECHNIQUES The proper selection of a fault isolation technique for a specific SRAM logic type failure requires an under- standing of available techniques. The most common and frequently used fault isolation techniques include: PEM, TIVA/ OBIRCH, CPA, and LVI/LVP. Among these diagnostic techniques, the PEM setup is the simplest, involving an optical microscope equippedwith a very sensitive photon detector (Fig. 1). PEM can pinpoint the defective location by detecting a very faint photon emission from the defec- tive circuit when a device under test (DUT) is electrically powered. Photon emission occurs as a result of the transi- tionof carriers fromahigher energy state toa lower energy state and is generally associated with forward or reverse biasedPN junctions, transistors in saturation, or dielectric breakdown. [7] Thus, the faults isolated by PEM are more likely to occur at the front end of line (FEOL), except for the case of a floating gate, which can be due to an open fault in the back end of line (BEOL).
Made with FlippingBook
RkJQdWJsaXNoZXIy MjA4MTAy