February_EDFA_Digital
edfas.org ELECTRONIC DEVICE FAILURE ANALYSIS | VOLUME 20 NO. 1 This is overcome with a high-speed digitizer capturing all the triggers for a short-loop acquisition time improvement of more than 50 × , even up to 500 × faster than a LeCroy oscilloscope. A 2 GHz bandwidth digitizer is 12 bits. For slow loops, high-bandwidth oscilloscopes are noisy. The digitizer allows for logic analysis in real-time, and binary searches are supported. The fifth presentation, “Visible versus IR for Laser Probing,” was given by Neel Leslie (Thermo Fisher Scien- tific, Fremont, Calif.). Laser voltage probing and laser voltage imaging directly expose electrical functionality of an IC or cell. The interplay between optical spatial resolu- tion (inversely proportional to wavelength) and transmis- sion through the silicon has necessitated near-infrared wavelengths (1064 to 1340 nm). Visible light probing has shown improved resolution (1320 to 785 nm, resolution improves 40%); however, trade-offs exist with laser inva- siveness and silicon thinning. To use the technique, silicon must be thinnedbelow10 µm. However, the impact of laser invasiveness on the measurements is still a question, but it can be reduced by lower laser power, less than 2 mW. At 5 µm silicon thickness, the transmission is 60%. The final presentation, “Techniques for Successful Backend-of-Line Nanoprobing,” was given by Weston Hearne (Thermo Fisher Scientific, Richardson, Texas). Electron beam induced resistance change (EBIRCH) and electron beam absorbed current (EBAC) for back-end-of- line (BEOL) fault localization have become significant use cases for nanoprobing. Fifty percent of nanoprobing is for BEOL EBAC/EBIRCH, but frontside EBAC/EBIRCH accounts for 90% and backside EBAC/EBIRCH for 10%. With EBAC, nets remain intact. This year the Contactless Fault Isolation and Nano- probing User Groups were combined into a single User Group meeting. The User Group had six presentations focusing on topics in both contactless optical probing and nanoprobing areas. All presentations were well received, with follow-on discussions and questions and answers during and after each presentation. Each of the presenta- tions showcased innovations in the contactless probing and nanoprobing areas and showed how the industry is moving forward to meet the challenges of semiconductor failure analysis today. More than 50 people attended the User Group meeting, and we look forward to a great 2018 User Group meeting as well. The organizers wish to thank Semicaps for their sponsorship of the session. ISTFA 2017 SAMPLE-PREP/3-D PACKAGE-PREP USER GROUP Moderators: Nathan Bakken, Intel Corp., and Tim Hazeldine, ULTRA TEC nathan.j.bakken@intel.com , tim@ultratecusa.com T he Sample-Prep User Group, sponsored by Varioscale, Inc., hosted four technical presenta- tions toward the development of new capabilities in the laboratory. The first presentation discussed ultra- flat repackaging as an alternative strategy to address the increasing complexity of coefficient of thermal expansion mismatch and other packaging-induced strains. The next two presentations addressed case studies where alterna- tive deprocessing techniqueswere successful for particular current and proposed applications. The final presentation reviewed workflows to assemble or reassemble multiple chip packages to enable physical debug workflows. The session was concluded by an interactive discussion where the audience engaged topublishananswer to the question: “What are the greatest challenges facing 3-D ICpackage and sample-preparation technologists until 2022?” “RapidRepackaging of Die for Backside Physical Failure Analysis” was presented by Scott Silverman of Varioscale, Inc. The presentation noted the benefits of backside silicon deprocessing methodology that are becoming increas- ingly threatened by a packaging roadmap that continues to include thinner and less rigid substrate materials. In addition to more complex shapes caused by the package roadmap, the requirement for thinner silicon found in Z -height constrained applications or to reduce backside absorption also benefits from highly planar samples. A video was provided to show the implementation of an electrically or optically initiated foil soldering solution that has been successful in preventing thermal damage andwas used to achieve surface flatness after mounting in the sub-100-nm range for an ~8 mm × 8 mm die. Also dis- cussedwas the selection of carrier materials to potentially S - 5
Made with FlippingBook
RkJQdWJsaXNoZXIy MjA4MTAy