edfas.org ELECTRONIC DEVICE FAILURE ANALYSIS | VOLUME 20 NO. 1 4 EDFAAO (2018) 1:4-8 1537-0755/$19.00 ©ASM International ® FAILURE MECHANISMS OF ELECTROMECHANICAL RELAYS ON PCBAs: PART I Gert Vogel, Siemens AG, Digital Factory Division, Control Products, DF CP QM SQA 5 gert.vogel@siemens.com INTRODUCTION Many printed circuit board assemblies (PCBAs) have relays that are soldered to the PCB. If such an electro- mechanical component fails, it can cause the whole device to fail, just like any other electronic component. The spectrum of root causes that lead to an increased contact resistance or a complete contact failure is totally different from what usually occurs in the electronics domain. This article provides a detailed analysis of these failures and the corresponding root causes, many of them self-centering. In this overview about failure mechanisms of electro- mechanical relays, the failure analysis discussed and the corresponding root causes are limited to contact failures between two contacts in relays that are used to switch small loads (Fig. 1). The relay has five terminals. The two terminals on the left in Fig. 1 arewired to a coil that creates a magnetic field when a current is applied. The magnetic field moves the middle contact of the three terminals on the right in Fig. 1, which connects or disconnects to the left and right contact. Nickel/silver or silver/tinoxide is usedas Fig. 1 X-ray of a common electromechanical relay. If an electric current is passed through the coil, it generates a magnetic field that activates the hinged armature on the left. Themovement is transferred to a plastic slider, and themovable contact—here in the middle of the three contacts—either opens (normally closed) or closes (normally open) a connection with the fixed contacts leftand right. Thepins are soldered to the PCB. Fig. 2 (a) Plastic chip from an edge of the plastic part. (b) Flux particle from a remote solder joint. (c) Solid plastic chip from a plastic part. (d) Flattened plastic particle exactly in the middle of the contact point the contactmaterial. Sometimes they are gold plated, but the failuremechanisms are incidental in the cases shown.

RkJQdWJsaXNoZXIy MjA4MTAy