Fall/Winter 2020 Catalog

5 FALL / WINTER 2020 CATALOG Elements of Metallurgy and Engineering Alloys gives a thorough presentation of physical and mechanical metallurgical concepts along with a practical survey of all important metals, their alloys, and their engineering properties. It covers basic metallurgy, metallic material selection, and application. The History of Metals in America chronicles the development of metals as both an industrial activity and a science. Progress involving structural metals made possible the air, land, sea, and space travel of today, skyscrapers reaching over 100 stories high, and many other engineering accomplishments that continue to shape modern society. Metallurgy for the Non-Metallurgist™, Second Edition provides a modern view of the basic principles and current practices of metallurgy. Recommended for anyone who uses, makes, buys or tests metal products. Answer all your basic metallurgy questions by using this updated reference featuring many illustrations, examples, and descriptions. Alloying: Understanding the Basics Edited by J.R. Davis • 2001 • 647 pages ASM Digital Library: $49 / ASM Member: $39 EISBN: 978-1-62708-297-6 Print: $187 / ASM Member: $135 ISBN: 978-0-87170-744-4 Product Code: 06117G ASM Metals Reference Book, Third Edition Edited by M.L. Bauccio • 1993 • 614 pages Print: $167 / ASM Member: $125 ISBN: 978-0-87170-478-8 Product Code: 06118G Dictionary of Metals Edited by Harold M. Cobb • 2012 • 374 pages Print: $157 / ASM Member: $115 ISBN: 978-1-61503-978-4 Product Code: 05359G Elementary Materials Science By William F. Hosford • 2013 • 188 pages ASM Digital Library: $25 / ASM Member: $17 EISBN: 978-1-62708-283-9 Print: $83 / ASM Member: $65 ISBN: 978-1-62708-002-6 Product Code: 05373G Elements of Metallurgy and Engineering Allo ys Edited by F.C. Campbell • 2008 • 672 pages ASM Digital Library: $49 / ASM Member: $39 EISBN: 978-1-62708-251-8 Print: $157 / ASM Member: $115 ISBN: 978-0-87170-867-0 Product Code: 05224G The History of Metals in America By Charles R. Simcoe, Edited by Frances Richards • 2018 • 256 pages ASM Digital Library: $25 / ASM Member: $17 EISBN: 978-1-62708-287-7 Print: $115 / ASM Member: $86 ISBN: 978-1-62708-145-0 Product Code: 05925G Joint EPRI-123HiMAT International Conference on Advances in High-Temperature Materials Edited by John Shingledecker and Masao Takeyama • 2019 • 1545 pages Print: $187 / ASM Member $135 ISBN: 978-1-62708-271-6 Product Code: 06026G Lightweight Materials: Understanding the Basics Edited by F.C. Campbell • 2012 • 720 pages ASM Digital Library: $49 / ASM Member: $39 EISBN: 978-1-62708-307-2 Print: $187 / ASM Member: $135 ISBN: 978-1-61503-849-7 Product Code: 05355G Materials and Coatings for Medical Devices: Cardiovascular 2009 • 452 pages Print: $307 / ASM Member: $231 ISBN: 978-1-61503-000-2 Product Code: 05269G A “MUST-HAVE” READY REFERENCE ONMETALLURG Y! Metallurgy for the Non-Metallurgist™, Second Editio n Edited by Arthur C. Reardon • 2011 • 526 pages ASM Digital Library: $49 / ASM Member: $39 EISBN: 978-1-62708-261-7 Print: $199 / ASM Member: $149 ISBN: 978-1-61503-821-3 Product Code: 05306G Transformations: Selected Works of G.B. Olson on Materials, Microstructure, and Design Edited by Carelyn E. Campbell, Michele V. Manuel, and Wei Xiong 2017 • 547 pages Print: $149 / ASM Member: $129 ISBN: 978-1-62708-137-5 Product Code: 06838G BEST SELLER! Worldwide Guide to Equivalent Irons and Steels, Fifth Edition 2006 • 1416 pages Print: $307 / ASM Member: $231 ISBN: 978-0-87170-822-9 Product Code: 05121G Worldwide Guide to Equivalent Nonferrous Metals and Alloys, Fourth Edition 2001 • 1036 pages Print: $307 / ASM Member: $231 ISBN: 978-0-87170-741-3 Product Code: 06735G SET SALE! Save up to $67 Worldwide Guide 2-Volume Set Print: $547 / ASM Member: $405 Product Code: 05192G MATERIALS AND ENGINEERING REFERENCE

RkJQdWJsaXNoZXIy MjA4MTAy