ADDITIVE BRAZING 13 ADDITIVE BRAZING FOR NEW PART PRODUCTION, REMANUFACTURING, AND WEAR PROTECTION Ino Rass and Timo Kolberg Euromat GmbH, Baesweiler, NRW, Germany Additive brazing produces dense, wear-resistant, crack-free, and corrosion-resistant coatings that often do not require further processing.