56 ASM NEWS The latest news about ASM members, chapters, events, awards, conferences, affiliates, and other Society activities. REVIEW OF NTSB INVESTIGATIONS OF CESSNA 210 HYDRAULIC ACTUATOR FRACTURES FROM FATIGUE Erik M. Mueller, Zoë Keliher, and Timothy Sorensen A persistent failure of main landing gear systems on a series of noncommercial planes was studied at the National Transportation Safety Board’s Materials Laboratory, leading to the discovery of cracks that propagated under cyclic loading of hydraulic actuators. 13 ADVANCED MATERIALS & PROCESSES | APRIL 2025 2 Single engine airplane flying at sunset through a sea of clouds. Courtesy of Dreamstime. On the Cover: 60 ASM STRATEGIC VISION ASM International is focused on fostering strategic collaborations, driving member engagement, and strengthening core foundations. AEROMAT SHOW PREVIEW The 36th AeroMat Conference and Exposition runs from May 6 to 8 in Vancouver, Canada. Photograph by Kristopher Grunert. 28