44 IMAT 2024 SHOW PREVIEW IMAT—the International Materials, Applications & Technologies Conference and Exhibition—and ASM’s annual meeting will be held in Cleveland, September 30 to October 3. EXPLORING THE TENSILE-COMPRESSIVE ASYMMETRY OF TITANIUM SAMPLES MADE BY WIRE ARC DIRECTED ENERGY DEPOSITION Blanca Palacios, Tanaji Paul, Arvind Agarwal, and Sean Langan This entry won first place in the light microscopy category of the prestigious 2023 International Metallographic Contest. 11 ADVANCED MATERIALS & PROCESSES | SEPTEMBER 2024 2 Optical micrograph of deformed profilometry-based indentation plastometry sample using polarized light and DIC microscopy. On the Cover: 62 ASM NEWS The latest news about ASM members, chapters, events, awards, conferences, affiliates, and other Society activities. ASM REFERENCE PUBLICATIONS & DIGITAL DATABASES CATALOG Our vast, authoritative reference library offers the most comprehensive and up-to-date materials information. 27