ADVANCED MATERIALS & PROCESSES | SEPTEMBER 2024 1 1 This entry won first place in the light microscopy category of the prestigious 2023 International Metallographic Contest. *Member of ASM International EXPLORING THE TENSILE-COMPRESSIVE ASYMMETRY OF TITANIUM SAMPLES MADE BY WIRE ARC DIRECTED ENERGY DEPOSITION LIGHT MICROSCOPY Blanca Palacios,* Tanaji Paul,* and Arvind Agarwal, FASM* Florida International University, Miami Sean Langan Solvus Global, Worcester, Massachusetts