35 2023 ASM FOUNDATION ANNUAL REPORT ASM’s Materials Education Foundation aims to inspire young people to pursue careers in materials, science, and engineering. UPCYCLING OF MIXED ALUMINUM ALLOY SHREDDER SCRAP USING SHEAR PROCESSING Brian Milligan, Scott Taysom, Ben Schuessler, Tim Roosendaal, Teresa Lemmon, and Scott Whalen Scientists at Pacific Northwest National Laboratory won an R&D 100 Award in 2020 for their advanced manufacturing technology, ShAPE, which reduces embodied energy as well as carbon when processing aluminum scrap. 15 ADVANCED MATERIALS & PROCESSES | JULY/AUGUST 2024 2 Artist Alicia Vasquez paints a park bench made from recycled wind turbine blades. Courtesy of Canvus. On the Cover: 59 ASM NEWS The latest news about ASM members, chapters, events, awards, conferences, affiliates, and other Society activities. IMAT 2024 PROGRAM HIGHLIGHTS IMAT—the International Materials Applications & Technologies Conference and Exhibition—and ASM’s annual meeting will be held in Cleveland, Sept. 30 to Oct. 3. 33