1 9 A D V A N C E D M A T E R I A L S & P R O C E S S E S | N O V E M B E R / D E C E M B E R 2 0 2 2 *Member of ASM International CONVENTIONAL LIGHT MICROSCOPY REVEALS BEAUTY OF SINGLE PHASE CARTRIDGE BRASS Grace A. Rome, Addison C. Wong, Carmen M. Sanchez, Gregory D. Vigil, W. Preston Cole II, Jason Yu, Robert S. Crow IV, and Gerald R. Bourne* Colorado School of Mines, Golden J A C Q U E T - L U C A S AWA R D 1 This entry won the prestigious Jacquet-Lucas Award for Best in Show at the 2021 International Metallographic Contest.