July/August_AMP_Digital
        
 SHOW PREVIEW September 15-16  |  Cleveland, Ohio The North American Cold Spray Conference is a returning highly successful ASM Thermal Spray Society event. Bringing together cold spray experts from around the globe, the 2020 conference will cover topics such as additive manufacturing; applications—case studies, cost analysis and optimization; equipment and quality control; fundamentals: physics, science, modeling and characterization; and the science and engineering of powders. Attendees will gain technical insight on new technology, exciting applications, and cutting-edge research. For more information and to register, visit  coldsprayevent.org . ASM International has been monitoring the development of COVID-19 and assessing its possible impacts on all of our organizations’ activities. We particularly consult with the Centers for Disease Control and Prevention (CDC) website, the World Health Organization (WHO) website and our local partners and government. As of today, the event will remain on schedule. To check up-to-date information, visit the Cold Spray site listed below or contact  events@asminternational.org . This year’s conference will include invited presentations by the following prominent speakers from industry, government, and academia: Richard Chromik, McGill University Cold-Sprayed Metal Matrix Composites for High Temperature Wear Applications Jan Cizek, Brno University of Technology Cold Sprayed W and W-CR Coatings for Fusion Applications Sophie Costil, Université de Technologie de Belfort Montbéliard Metallization of CFRC and PEEK Polymers using Cold Spraying: Suitable Conditions for Increasing the Deposition Eiciency Reza Daroonparvar, ASB Industries Inc. Applying Zr702 Layer on Commercially Pure Aluminum Coated Magnesium Alloy using Cold Spray Process Terry Gabbert, USAF Life Cycle Management Center (LCMC) Status of Cold Spray in the Air Force Jean-Philippe Gagnon, Telops Cold Spray Measurements: A Brief Presentation Mario Guagliano, Politecnico di Milano From Repair to Additive Manufacturing: The Fatigue Challenge of Cold Spray Mostafa Hassani, Cornell University In-Situ Synchrotron X-ray Studies of the Mechanics of Cold Spray Composites Aleš Herrmann, SAFINA CGS for Jumbo Sputtering Target Production Eric Irissou, National Research Council Cold Spray Additive Manufacturing and Structural Repair of Steels Kelvin Bi Jiawei, Republic of Singapore Air Force Cold Spray Repair of Lightning-strike Damaged Aircra Winglet Bertrand Jodoin, University of Ottawa Hybrid Induction Heating Cold Spray as Potential Additive Manufacturing Technology Peter King, CSIRO: Commonwealth Scientific and Industrial Research Organization Cold Spray as an Additive Manufacturing Process Thomas Klassen, Helmut Schmidt University Kinetic Spraying of Materials with Limited Ductility Heli Koivuluoto, Tampere University of Technology Diagnostics and Characterization of Cold-sprayed Metallic Coatings for Repairing Applications Jussi Larjo, Oseir-SprayWatch Online Monitoring Solutions for Cold Spray Processes Rocco Lupoi, Trinity College, Dublin Towards the Development of a Hybrid Additive Manufacturing Process: How Cold Spray and Selective Laser Melting Can Work Together André McDonald, FASM, University of Alberta Microstructure-Dependency of Mechanical Properties and Failure of Low-Pressure Cold-Sprayed Tungsten Carbide-Nickel Metal Matrix Composite Coatings Alexandre Nadeau / Olivier Duchesne, Tecnar Automation Ltée. Novel Sensor for Cold Spray Processes In-Flight Particle Diagnostics Luc Pouliot, Polycontrols Technologies Production Process for Cold Spray Cu-based Anti-Microbial Coatings Applied to High-Touch Surfaces in Public Spaces Peter Richter, Jr., Impact Innovations GmbH Advancements in Cold Spray Gobinda Saha, University of New Brunswick Engineered Cermet Feedstock Powder Development for High-pressure Cold Spray Additive Manufacturing Harpreet Singh, Indian Institute of Technology Ropar Strategies to Improve Adhesion Strength of Cold-Sprayed Coatings Kumar Sridharan, FASM, University of Wisconsin Cold Spray Technology in Nuclear Energy Applications Oliver Stier, Siemens Aordable Cold Spray Julio Villafuerte, SST Centerline Ltd. The Evolution of the Implementation of Cold Spray Technology Across Various Commercial Applications Since the 1990s Christian Widener, VRC Metal Systems Emerging Industrial Opportunities for Cold Spray coldsprayevent.org SPONSORED BY: ORGANIZED BY:
        
         Made with FlippingBook 
RkJQdWJsaXNoZXIy MjA4MTAy