A D V A N C E D M A T E R I A L S & P R O C E S S E S | A P R I L 2 0 2 0 4 8 iTSSe TSS iTSSe TSS Figure 6 shows the wear behavior of the PS 304 coating, exhibiting sporadic wear spikes and unsteady wear track. There appears to be an intermittent transfer film buildup on the pin from the worn coated disc, leading to spikes on the wear track. Overall, the Triboglide coating shows excellent wear and friction properties compared to the commercially available PS 304 coating. ~iTSSe Fig. 6 — High temperature pin-on-disc testing of NASA PS 304 coating. For more information: Satish Dixit, Plasma Technology Inc., 1754 Crenshaw Blvd., Torrance CA 90501, 860.282.0659, www. ptise.com . FEATURE 14