May/June_AMP_Digital
FEATURE A D V A N C E D M A T E R I A L S & P R O C E S S E S | M A Y / J U N E 2 0 1 8 4 0 9 Fig. 4 — Cooling curves and temperature gradients for all air quenching configurations. Fig. 5 — High-temperature gradient locations for conveyer quenching (Fig. 3a) and basket quenching (Fig. 3d), 60 seconds into quenching. Fig. 6 — Experimental setups and CFD simulations for water quenching cylinder blocks; cooling curves from simulations and thermo- couple measurements plotted together for comparison. 8