April_AMP_Digital

A D V A N C E D M A T E R I A L S & P R O C E S S E S | A P R I L 2 0 1 8 1 6 SURFACE ENGINEERING SLIP AND SLIDE COATING RESISTS FOULING Since the banning of toxic tribu- tyltin, demand is mounting for environ- mentally friendly methods to prevent marine fouling, and scientists from the University of Sydney Nano Institute, Australia, have responded with a new surface coating that uses nanostructur- ing—not toxins—to prevent bio-build- up. The coating incorporates nano- wrinkles modeled on the tiny structures around the rim of the carnivorous Ne- penthes plant that trap water, creating a slick surface that sends insects sliding into the plant’s pitcher to be digested. Similarly, the new coating creates a slippery surface that prevents initial adhesion of bacteria, thereby inhib- iting formation of biofilms, which are a precursor to the buildup of fouling organisms. In the lab, surfaces treated with the new coating resist almost all fouling from a common species of marine bac- teria, while control Teflon samples are completely fouled. When test surfaces were attached to swimming nets at Watsons Bay baths in Sydney Harbor for a period of seven weeks, the sur- faces with the new coating were very efficient at resisting fouling. The new coatings are moldable and transpar- ent, making their application suitable for underwater cameras and sensors. In addition, their slippery surface could reduce drag on marine vessels, upping energy efficiency. www.sydney.edu.au . COATING KEEPS COOL UNDER FIRE Researchers from Nanyang Tech- nological University and industrial developer JTC, both in Singapore, in- vented a new fire protection coating for steel building structures that is 50% more cost effective to apply than con- ventional intumescent coatings. The new paint, called FiroShield, requires just five layers to achieve a standard two-hour fire rating—enough time for building occupants to evacuate—while conventional coatings can require more than 15 layers for similar protection. In addition, because sand blasting is not The Nepenthes pitcher plant traps a lubricating layer in the structure of its peristome. Newly developed nanowrinkles work the same way, trapping a lubricating layer that stops the adhesion of bacteria and other marine organisms. required to prepare a surface for Firo- Shield, overall application time and related labor costs are reduced by half. The paint’s superior performance can be ascribed in part to a unique endo- thermic ingredient that absorbs heat from a fire, triggering a chemical reac- tion that causes the coating to adhere more firmly to the steel. “In a fire, our coating forms a com- pact charred layer that acts as a protec- tive barrier,” explains assistant profes- sor Aravind Dasari. “While typical fire coatings will also form a charred layer, those are thick and foam-like, which can fall off easily and leave the steel exposed.” In addition, the new coating provides corrosion protection—some- thing no other fire coating currently offers—and withstands weathering. In lab tests, its performance barely dipped by 2% when subjected to weathering, while conventional coatings showed up to a 75% performance drop. FiroShield meets similar performance standards when applied to construction materials such as reinforced concrete and lami- nated timber, and it can even be tinted like traditional paint. www.ntu.edu.sg , jtc.gov.sg . BRIEF AkzoNobel, the Netherlands, donated more than 1600 gallons of military-grade International Marine Coating to repaint the 873-ft USS Hornet Sea, Air & Space Museum docked in Alameda, Calif. Decommissioned in 1970, the USS Hornet was named a National Historic Landmark in 1991 and was converted into a museum in 1998. The new paint job will allow museum visitors to see what the Hornet looked like when it was commissioned in 1943. akzonobel.com . USS Hornet Sea, Air & Space Museum. Scientists fromNanyang Technological University and JTC display steel plates coated with different shades of FiroShield.

RkJQdWJsaXNoZXIy MjA4MTAy