edfas.org ELECTRONIC DEVICE FAILURE ANALYSIS | VOLUME 20 NO. 2 26 RECENT INNOVATIONS IN EX SITU LIFT OUT APPLICATIONS AND TECHNIQUES Lucille A. Giannuzzi EXpressLO LLC, Lehigh Acres, Fla. lucille.giannuzzi@expresslo.com EDFAAO (2018) 2:26-32 1537-0755/$19.00 ©ASM International ® INTRODUCTION The ability to apply focused ion beam (FIB) milling to just about any material for site-specific scanning/ transmission electron microscopy (S/TEM) was realized in the mid 1990s to early 2000s. The first technique used to extract or “lift out” site-specific FIB milled specimens, now commonly referred to as “ex situ lift out” (EXLO), also proved successful formany differentmaterials. [1-4] With the EXLO method, specimen extraction is performed outside of the FIB instrument (i.e., not with an in situ probe) using a light optical microscope andmicromanipulator station. The semiconductor industry immediately embraced EXLO and continues to rely on this technique due to its ease of use, reproducibility, and high throughput. For example, it is possible to lift out and manipulate 20 specimens (or more) per hour using EXLO. [5] The EXLO technique relies on the physics of adhesion forces, and more specifically, van der Waals forces (i.e., not electrostatic forces as previously believed) to transfer a FIBmilled speci- men confined within its trench to a specimen carrier using a glass probe micromanipulator. [6] S/TEM EXLO specimens are usually manipulated to carbon, formvar, or holey carbon coated 3-mm grids or similar. In addi- tion, S/TEM EXLO specimens can also be manipulated to MEMS devices for heating, electrical, or other in situ S/TEM observation of materi- als, [6,7] or more recently, to slotted half-grids. [6] The slotted half-grids allow additional processing of EXLO specimens, suchas FIBmilling for back- side thinning, including low energy FIB or ion mill- ing. [6,8-9] These innovations and advances in EXLO are detailed below. EXLO AND VAN DER WAALS FORCES As previously shown, [6] the EXLO method relies on adhesion forces, and specifically van der Waals (VDW) forces, topick up a specimen andmanipulate it to a carrier of choice. Figure 1 compares the adhesion forces and the force of gravity acting on a typical Si FIB specimen with dimensions of 10 µm × 5 µm × 100 nm and a glass probe manipulator pulled to 2 µm in diameter. Glass probes are typically used because they are inexpensive, easy to prepare, and flex without deforming during the lift out and manipulation process. A single glass needle may be used to manipulate tens of samples or more. As shown in Fig. 1 Comparisonof adhesion forcesand forceof gravityactingonaSi FIBspecimen 10 µm × 5 µm × 100 nm.

RkJQdWJsaXNoZXIy MjA4MTAy