February_EDFA_Digital
edfas.org ELECTRONIC DEVICE FAILURE ANALYSIS | VOLUME 20 NO. 1 Demonstrated tests included 1.8 nm resolution at 10 kV/1 pA, low invasiveness in a chip edit simulation, excellent imaging and nanomachining control, and ultrafast second- ary ion mass spectrometry (SIMS) acquisition. Sharang, from Tescan Orsay, presented the second talk, “Delayering Capabilities Using Xe + Plasma FIB and Associated In Situ Nanoprobing Operations.” He began by showing impressive delayering results from the M4 metal layer down to gates over a 40 × 40 µm area on a popular 14 nm FinFET processor product. The resulting surface roughness, as measured by atomic force microscopy tech- nology, was very low, which enabled easy in situ nanoprob- ing at the individual FinFET transistor level. Results were shown from an eight-tip stage-mounted prober assembly and even an in situ atomic force probe. However, being able toplasma-FIBdeprocess the upper levels (thick, wide, and not necessarily fully planarized) would normally require starting with highly inexact mechanical parallel polishing. The trick shownwas tobegin the process on flip-chip module-mounted dice, as though it was the start of an FIB chip edit. Sharang began with ultrathin CNC contour milling followed by XeF 2 clearing of all remaining silicon to the underside of the finmandrel and shallow trench isolation regions. Planar deprocessing then proceeded, using a proprietary gas and Xe + beam process through the thin lower interconnects and into the thicker layers from the bottom side upward. Michael DiBattista from Varioscale presented “A Decision Tree for FIB Sample-Preparation Strategy.” The idea for this talk came from a lunchtime discussion some months ago about all the possible options available to those engaged in FIB chip circuit edit. Depending on the tools at one’s disposal, time issues, edit-site peculiarities or the need to do multiple edits, and customer requirements (systemuse or test with or without probing), onemay have either a clear choice or multiple possible paths. These include, but arenot limited to, localizedorwide-areapartial or full-thickness silicon trenching (laser chemical etching, plasma FIB, or FIB XeF 2 ) or mechanical prethinning (local- ized pocket, moderate thickness remainingwith or without contour following, or ultrathin silicon remaining). The need for good end-pointing and variousmethodswere explored. From the “nuclear option” to ultrathinning, Mike stepped through each scenario and suggested the best toolset to use to achieve individual sample-prep needs. Valery Ray of PBS&T, MEO Engineering/University of Connecticut, presented the fourth paper, “Quantifiable Comparative Evaluation of FIB/SEM Instruments.” Valery discussed the need to design quantifiable evaluation tests for FIB systems, noting that “canned” demos are designed to exploit the best features of a given tool but not necessar- ily show the full picture of the tool. He showed examples of standardized samples and a number of qualification tests, including beamburns, current versus dose, drift tests, patterning performance tests, and imaging tests. He also suggested some customized combination tests that will emulate specific-use cases. Being preparedwith one’s own evaluation suite that can be performed on all FIBplatforms under consideration will help end-users make the best tool-purchasing decision. The fifth paper, “Sub-Pico-Amp Focused Ion Beam (FIB) for Circuit Edit on FinFET Technology,” was given by Hideo Tanaka from FEI/Thermo Fisher Scientific. Hideo’s talk explored the challenges that are arising from shrinking process nodes that accompany the adoption of FinFET technology. He stressed that a circuit edit solution which includes sub-pA beamcurrents, precisionmilling, and opti- mized gas and recipesmust be precise. Critical for meeting today’s chip edit challenges is an improved secondary- electron detector to be able to image the scant amount of signal for end-pointing and so on. He showed a case study of circuit edit work with emphasis on the key elements required to enable a successful, functional modification. The sixth and final paper of the workshop session, “Neon GFIS-Induced Chemical-Assisted Etch and Beam- Induced Deposition Characterization,” was presented by Rick Livengood of Intel. The first part of Rick’s talk included a reviewof neon gas field ion source (GFIS) technology and how it has been used for nanopatterning, surface analysis, transmission electron microscopy prep, and early circuit edit attempts. He noted that some of the key attributes to GFIS technology are that neon generates two to three times the secondary electron yield relative to gallium, and also, the sputter yield is half of gallium. That providesmore reaction time alongwith better visual and instrumentation end-pointing. The second segment included an update of recent experimental results comparing neon via sputtering versus gas-assisted neon etching, and deposition of oxides and metals using neon as the primary beam. Much of the work was done using a new gas system from Xidex that features dual opposing XeF 2 gas nozzles along with nozzles for an oxide source (PMCTS and oxygen). Overall, neon appears to address some of the limitations presented by gallium for chip edit andwill be a good complement as a dual-column system for use on sub-10-nm process nodes. S - 3
Made with FlippingBook
RkJQdWJsaXNoZXIy MjA4MTAy