130 YEARS OF ENGINEERED GRAPHITE: INVENTION TO INDISPENSABLE GRAPHITE DEVELOPMENT 15 Ryan M. Paul* GrafTech International Holdings Inc., Cleveland This historical review details the critical developments and evolving applications of graphite from the dawn of carbon materials to the space age and beyond. *Member of ASM International