ADVANCED MATERIALS & PROCESSES | JULY 2026 14 DAMAGE ASSESSMENT OF ANCIENT SILVER DISHES AND PLATES ARCHAEOMETALLURGICAL STUDY Russell Wanhill, Caligula University Emmeloord, the Netherlands Omid Oudbashi,* University of Gothenburg, Sweden Recovered ceremonial plates from the late Roman and early Byzantine periods are noninvasively examined to investigate damage that occurred both prior to their burial in the 5th-6th centuries and as a result of it. *Member of ASM International